Patents
US 4,459,779 A#847765 Most CitedExpiredUnited States (USPTO)Utility

Fixed abrasive grinding media

53Forward Citations (#847765 Global)
1.3/yrCitation Velocity (#4673299 Global)
5.25Citation PageRank (#3058878 Global)
8Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The grinding media is formed of a concentration of agglomerate free hard particles exceeding 50 percent by weight of the media, wherein the particles are chelated by a dispersing agent, surface treated with a surfactant, mixed with polyether polyol and polyisocyanate plus a catalyst and water and thereafter rapidly cured in a closed mold which has been preheated to a temperature exceeding 50° C. and a pressure of 60 to 120 PSIG. The water reacts during curing to create a polyurea linkage and release CO 2 as a blowing agent. The resulting media has a low elastic modulus with particles retained in a polyurethane-urea binder system. The media composition may also include an inorganic filler such as glass fibers not exceeding 30 percent by weight of the media.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 53.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    The method of fabricating an abrasive grinding media comprising: mixing classified abrasive particles which have been surface treated with a dispersing agent and from which agglomerates have been removed with multifunction, low viscosity polyether polyol; multi function polyisocyanate; water and a catalyst; placing the mixture in a mold which has been preheated to 40° to 70° C.; pressurizing the mold cavity to 60 to 120 pounds per square inch; and curing at a temperature of at least 150° C., whereby a fast reaction occurs at conditions of elevated temperature and pressure to produce a mi

  2. Claim 2Depends on #1

    The method of claim 1 wherein said mixing step further comprises the addition of a surfactant and said curing step occurs at a temperature of from 150° to