Patents
US 4,459,153 A#17469435 Most CitedExpiredUnited States (USPTO)Utility

Pyrochemical process for extracting plutonium from an electrolyte salt

6Forward Citations (#17469435 Global)
0.1/yrCitation Velocity (#39251188 Global)
1.70Citation PageRank (#18731859 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A pyrochemical process for extracting plutonium from a plutonium-bearing salt is disclosed. The process is particularly useful in the recovery of plutonium from electrolyte salts which are left over from the electrorefining of plutonium. In accordance with the process, the plutonium-bearing salt is melted and mixed with metallic calcium. The calcium reduces ionized plutonium in the salt to plutonium metal, and also causes metallic plutonium in the salt, which is typically present as finely dispersed metallic shot, to coalesce. The reduced and coalesced plutonium separates out on the bottom of the reaction vessel as a separate metallic phase which is readily separable from the overlying salt upon cooling of the mixture. Yields of plutonium are typically on the order of 95%. The stripped salt is virtually free of plutonium and may be discarded to low-level waste storage.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of extracting plutonium from an electrolyte salt containing dispersed particles of plutonium metal, comprising the steps of: forming a mixture of said electrolyte salt with metallic calcium in a reaction vessel; heating said mixture until said salt is molten, and stirring the molten salt to effect reduction and coalescence of plutonium in said salt to a separate molten metallic plutonium phase; and cooling said mixture and mechanically separating said metallic plutonium phase from said salt.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the amount of calcium is between approximately 30 and 350 grams of calcium per kilogram of plutonium contained in said salt.

  3. Claim 3Depends on #2

    The method of claim 2 wherein the amount of calcium is on the order of 90 grams of calcium per kilogram of plutonium contained in said salt.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Mullins et al., "A Review of Operating Experience at the Los Alamos Plutonium Electrorefining Facility, 1963-1977," LA-8943, Dec. 1981.
  • Mullins et al., "Fused Salt Processing of Impure Plutonium Dioxide to High-Purity Plutonium Metal," LA-9154-MS UC-10, Jan. 1982.
  • Mullins et al., A Review of Operating Experience at the Los Alamos Plutonium Electrorefining Facility, 1963 1977, LA 8943, Dec. 1981.
  • Mullins et al., Fused Salt Processing of Impure Plutonium Dioxide to High Purity Plutonium Metal, LA 9154 MS UC 10, Jan. 1982.