Patents
US 4,457,785 A#1331828 Most CitedExpiredUnited States (USPTO)Utility

Treated glass fibers and nonwoven sheet-like mat and method

41Forward Citations (#1331828 Global)
1.0/yrCitation Velocity (#7467741 Global)
6.89Citation PageRank (#1964106 Global)
18Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Treated glass fibers are provided that are more dispersible in aqueous media. The glass fibers are treated with a composition having a nonionic surfactant and a cationic quaternary ammonium salt surfactant. The composition may be added simultaneously or sequentially with the chopped glass fibers to the aqueous media in which the glass fibers are to be dispersed. Also, glass fibers can be treated with an aqueous treating composition having the composition and produced into wet or dry chopped glass fibers having a length of about 1/16 of an inch to about 3 inches. The treated glass fibers have good dispersibility in aqueous media with or without the addition of dispersing agents.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 41.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Method of dispersing chopped glass fibers in aqueous media, comprising: (a) adding to the aqueous media in which the glass fibers are to be dispersed about 10 to about 500 parts per million (PPM) of the aqueous media of a blend of a nonionic surfactant and cationic quaternary ammonium salt surfactant where the ratio of the nonionic to cationic surfactant is about 1 to about 99 to about 99 to about 1, and (b) adding sized or unsized chopped glass fibers to the aqueous media in an amount of about 0.001 to about 3 weight percent of the aqueous media, and (c) agitating the mixture to produce a

  2. Claim 2Depends on #1

    Method of claim 1, wherein the nonionic and cationic surfactants are used as a blend in a ratio of about 3:1 to about 1:3.

  3. Claim 3Depends on #1

    Method of claim 1, wherein the nonionic surfactant is selected f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (18)

PatentTitleYearCitations
US 3,850,869 AGlass fiber sizing composition and resultant product with high resistance to abrasion197416
US 3,869,308 AForming size for glass fibers and resulting product197532
US 3,997,306 AGlass fiber sizing composition for the reinforcement of resin matrices and method of using same197674
US 4,002,445 AMethod of forming and sizing glass fibers197718
US 4,052,256 AMethod of dispersing glass fibers using a linear polysiloxane and dispersion obtained thereby197712
US 4,052,257 AMethod of producing glass mats197731
US 4,110,094 AMethod of forming glass fiber197839
US 4,118,272 AContinuous wet-laid process for making high-strength glass fiber mats197829
EP 0,003,475 A1Manufacture of uniform glass mats by the wet-laid process, a glass-fiber dispersion used in this process and coated glass fibers—9
US 4,178,204 AWet-strength of wet glass fiber mats by treatment with anionic polyelectrolytes197918
US 4,178,203 AMethod of increasing the strength of wet glass fiber mats made by the wet-laid process197930
US 4,178,206 AMethod of forming glass fiber dispersions with cationic quaternary ammonium surfactants having at least two long chain groups197915
US 4,179,331 AGlass fiber dispersions for making uniform glass fiber mats by the wet-laid process197925
US 4,183,782 AMethod of producing glass mats using novel glass fiber dispersion composition198022
US 4,185,138 ASize composition and method of producing same to render glass fiber having improved dispersibility in aqueous solutions198018

Non-Patent Literature (2)

  • Amasoft P M Concentrate Product Bulletin.
  • Amasoft® P-M Concentrate Product Bulletin.