US 4,454,740 A#1463662 Most CitedExpiredUnited States (USPTO)Utility

Method for simultaneous peening and smoothing

39Forward Citations (#1463662 Global)
0.9/yrCitation Velocity (#7650354 Global)
5.47Citation PageRank (#2860511 Global)
4Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method for simultaneously shot peening and smoothing includes use of relatively large, smooth, hard, spherical steel shot having a substantially uniform diameter in the range 1-2.5 mm. Titanium workpieces are provided in one step with a compressive stress layer of the order of 0.13 mm and a surface finish of better than 15×10 -6 inch AA, compared to conventional peened finishes of the order of 40×10 -6 inch AA. Surface finish and peening intensity are inter-related and dependent on shot diameter, mass, velocity, and energy within relatively small limits. The shot diameter is uniform within ±0.05 mm; the shot impact velocity is uniform within ±4 percent or less, in the range 1.4-12 m/s.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 39.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method of surface treating a workpiece, to provide residual compressive stresses corresponding to a peening intensity of at least 0.1 mm N and a surface finish smoother than 40 microinch AA, characterized by impacting the workpiece surface with spherical shot particles, the shot particles being infrangible, having a hardness greater than the workpiece, a surface finish better than 30 microinch AA, and diameters lying in the range 1-2.5 mm which are substantially uniform to within at least ±5%.

  2. Claim 2Depends on #1

    The method of claim 1 wherein the shot particle masses are uniform within ±16%.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the shot particles have a velocity in the range 1.4-12 meters per second, uniform within ±4%.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • ASM "Shot Peening," Metals Handbook, vol. 2, pp. 398-405, (1964), Amer. Soc. for Metals.
  • ASM Shot Peening, Metals Handbook, vol. 2, pp. 398 405, (1964), Amer. Soc. for Metals.
  • Brandel, Klass "Ball Forming Solves Contouring Problems," Metal Progress, (Mar. 1971), pp. 56-57.
  • Brandel, Klass Ball Forming Solves Contouring Problems, Metal Progress, (Mar. 1971), pp. 56 57.
  • Carlin, "What Makes a Good Steel Shot", Metal Progress; Jun. '59; pp. 83-85.