Patents
US 4,454,085 A#3596297 Most CitedExpiredUnited States (USPTO)Utility

Process for producing asymmetrical hollow filament membranes of polyamide

22Forward Citations (#3596297 Global)
0.5/yrCitation Velocity (#15017361 Global)
5.29Citation PageRank (#3021723 Global)
12Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process is disclosed for the production of asymmetrical hollow filament membranes suitable for ultrafiltration and/or microfiltration, in which a spinning solution composed of a polyamide or a mixture of polyamides and/or copolyamides, formic acid and a coagulating core liquid, is extruded into a coagulating setting bath liquid, and the hollow filaments are stretched after leaving the setting bath, in the wet state. The pH-value-difference between core liquid and setting bath liquid should be at least 3. The spinning solution contains, in particular, 15 to 25% by weight polyamide, 5 to 20% by weight polyethylene glycol, up to 10% by weight customary additive and formic acid. Preferred embodiments include a stretching ratio amounting to between 1:1.5 and 1:2.5, and having core liquid and setting bath liquid chosen from various combinations of caustic soda, glycol, formic acid or polyethylene glycol. Also disclosed are hollow filament membranes in which the hollow filament is of uniform, eccentric or profiled shape.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 22.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    Process for the production of an asymmetrical hollow filament membrane suitable for ultrafiltration and/or microfiltration, comprising extruding a spinning solution composed of a polyamide or a mixture of polyamides and/or copolyamides with formic acid and a coagulating core liquid into a coagulating setting bath liquid different from the core liquid, stretching hollow filaments produced thereby, in the wet state, after leaving the setting bath and then drying the hollow filaments, wherein said spinning solution containing 15 to 25% by weight of polyamide, 5 to 20% by weight polyethylene glyco

  2. Claim 2Independent Claim

    Process a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗