Reduction of wall fouling in the suspension polymerization of vinyl chloride homopolymer
Abstract
This invention relates to a method for reducing the amount of wall fouling in the suspension polymerization of vinyl chloride. The surfaces of the polymerization reactor are wetted with a solution containing from 5 to 50 wt % alkali metal hydroxide, 0.01 to 1 wt % free radical inhibitor and 0.01 to 1 wt % surface active agent prior to charging the vinyl chloride polymerization recipe to the reactor. Preferably, the surface of the wetted reactor is heated to a temperature from 40° to 100° C. for at least 5 minutes prior to charging the polymerization recipe.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
In a suspension polymerization process wherein vinyl chloride monomer, water, a suspension agent and a monomer soluble polymerization catalyst is charged in stainless steel reactor at an initial pH above 6.0 and subsequently polymerized at an elevated temperature to produce a vinyl chloride homopolymer, the method for reducing wall fouling in the stainless steel reactor which comprises wetting the internal reactor surfaces with a solution consisting essentially of a solvent and (a) 5 to 50 wt % alkali metal hydroxide, (b) 0.01 to 1 wt % free radical inhibitor, and (c) 0.01 to 1 wt % surfac
- Claim 2Depends on #1
The invention of claim 1 which includes the step of heating the wet reactor surface to a temperature from about 40° to 100° C. for a period of at least 5 minutes prior to charging the polymerization components to the reactor.