Reaction injection molded elastomer using a methylene bis(phenyliscoyanate) containing 2,4' isomer in amounts greater than about 10 percent
Abstract
The invention is a method of making a molded reaction injection molded elastomer. The reaction injection molded (RIM) elastomer is made by injecting via a RIM machine into a mold cavity of the desired configuration, a formulation comprising in the first stream amine terminated polyethers of greater than 1,500 molecular weight, a chain extender, and in the second stream methylene bis(phenylisocyanate) with a 2,4' isomer of greater than about 10%. RIM elastomers are useful, for example, for automobile body parts.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 37.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method for making a reaction injection molded elastomer comprising injecting into a mold cavity of desired configuration, a formulation comprising primary or secondary amine terminated polyethers of greater than about 1,500 molecular weight wherein greater than 50% of the active hydrogens are in the form of amine hydrogens, an amine terminated chain extender and a methylene bis(phenylisocyanate) wherein the 2,4' isomer is present in amounts greater than about 10%.
- Claim 2Depends on #1
A method as in claim 1 wherein the amine terminated polyether has a functionality of about 2 to 6.
- Claim 3Depends on #2
A method as in claim 2 wherein the functionality of the amine terminated polyethers is from about 2 to 3.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗