Method of sizing hydrophobic yarn
Abstract
A method of sizing a hydrophobic yarn for weaving comprising the steps of applying thereto an acid pH latex of a free radical initiated vinyl polymer and drying the yarn. The polymer has a weight average molecular weight of from about 300,000 to about 2,500,000, and in dried film form is hydrophobic, not redispersible in a solution at a low pH and redispersible in an alkaline aqueous medium. The polymer is prepared from monomers comprising about 8% to about 14%, by weight ethylenically unsaturated acid. The average solubility parameter of the monomers in the polymer is between about 9.0 and about 9.5; the calculated polymer T g is between about -20° C. and 20° C. Preferred yarns are nylon and polyester.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 13.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of sizing a hydrophobic yarn for weaving comprising the steps of ( 1) applying thereto an acid pH latex of a free radical initiated vinyl polymer having a weight average molecular weight of from about 300,000 to about 2,500,000; said polymer, in dried film form, being hydrophobic and not redispersible in a solution at a low pH and being redispersible in an alkaline aqueous medium; said polymer being of monomers having a solubility parameter from about 9.0 to about 9.5, a T g from about -20° C. and comprising 8% to about 14%, by weight, alpha, beta-ethylenically unsaturated acid, and
- Claim 2Depends on #1
The method of claim 1, the yarn being of polyester or nylon, the polymer being of monomers selected from butyl acrylate, from styrene, acrylic acid, methacrylic acid, ethyl acrylate, 2 ethyl hexylacrylate, propyl acrylate and meth
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗