Centrifugally cast tube of spheroidal graphite cast-iron and its method of manufacture
Abstract
The cast tube (T) is subjected internally in a chill-mould (1) to the uniform spraying of water from 1000° C. approximately to 350° C. approximately. Then it is extracted from the chill-mould and in a furnace is subjected to isothermal bainitization maintenance, after which it is cooled in the atmosphere to ambient temperature. Without it being necessary to add expensive chilling elements, one thus obtains lightened tubes having very good mechanical properties and the ovalization of which remains acceptable.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 21.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Centrifugally cast tube of spheroidal graphite cast-iron, characterised in that the cast-iron has the following composition by weight: carbon: 2.5-4.0% silicon: 2-4.0% manganese: 0.1-0.6% nickel: 0-3.5% copper: 0-11% magnesium: 0-0.5% sulphur: 0.01% maximum phosphorus: 0.06% maximum the remainder being iron, this cast iron having a bainitic structure.
- Claim 2Depends on #1
Tube according to claim 1, characterised in that the cast-iron has the following composition: carbon: 3.6% silicon: 2.4% manganese: 0.5% nickel: 0.2% copper: 0.5% magnesium: 0.03% sulphur: ≦0.01% phosphorus: ≦0.06%, the remainder being iron.
- Claim 3Depends on #1, #2
Tube according to claims 1 or 2, characterised in that it corresponds to the following table: ______________________________________ Nominal