Patents
US 4,446,261 A#19973 Most CitedExpiredUnited States (USPTO)Utility

Process for preparation of high water-absorbent polymer beads

312Forward Citations (#19973 Global)
7.4/yrCitation Velocity (#104820 Global)
32.49Citation PageRank (#147563 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Water-insoluble, high water-absorbent polymer beads are prepared by dispersing and suspending an aqueous solution of a water-soluble, ethylenically unsaturated monomer containing a small amount of a crosslinking agent in a dispersion medium of a hydrocarbon or a halogenated aromatic hydrocarbon, carrying out the bead polymerization in the presence of a water-soluble radical polymerization initiator and a protecting colloid comprising a cellulose ester or cellulose ether which is oil-soluble at the polymerization temperature, and separating the resulting beads.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 312.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing beads consisting of water-insoluble, crosslinked polymer, which beads have a particle size of from 100 to 1000 microns and have an absorbent capacity for physiological saline in the range of from 30 to 150 grams per one gram of the dried polymer, which consists of the steps of: dispersing droplets of (1) an aqueous solution consisting of water-soluble, ethylenically unsaturated monomer, from 0.01 to 5% by weight, based on the weight of said monomer, of water-soluble crosslinking agent, a water-soluble radical polymerization initiator, and the balance is water, said aque

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗