US 4,444,718 A#9852391 Most CitedExpiredUnited States (USPTO)Utility

Method of making a high current density cathode

10Forward Citations (#9852391 Global)
0.2/yrCitation Velocity (#30245476 Global)
3.70Citation PageRank (#5398121 Global)
3Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A high current density cathode is made by first forming an active porous h purity tungsten pellet by the steps of: (A) mixing tungsten powder with about 1 to 5 percent by weight of the mixture of an activator powder and compacting the powders at a pressure of about 35 tons per square inch to form a pellet, (B) sintering the pellet in a non-oxidizing atmosphere at about 1800 degrees C. for about 11/2 to 31/2 hours to the desired porosity, (C) filling the porous pellet with a filler material, (D) machining to the desired size and shape, (E) removing the filler material, and then forming the cathode by impregnating the pellet with Ba 5 Sr(WO 6 ) 2 at about 1700 degrees C. in an inert atmosphere and subsequently firing for 2 minutes at 1800 degrees C. in dry hydrogen.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 10.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method of making an active porous high purity tungsten pellet, said method including the steps of: (A) mixing tungsten powder with about 1 to 5 percent by weight of the mixture of an activator powder selected from the group consisting of zirconium hydride, hafnium hydride, scandium oxide, yttrium oxide and aluminum oxide and compacting the powders at a pressure of about 35 tons per square inch to form a pellet, (B) sintering the pellet in a non-oxidizing atmosphere at about 1800 degrees for about 11/2to 31/2 hours to the desired porosity, (C) filling the porous pellet with a methyl methacr

  2. Claim 2Depends on #1

    Method according to claim 1 wherein the activator powder is zirconium hydride.

  3. Claim 3Independent Claim

    Method according to claim

Technical Overview & Description