Production of sodium hydroxide and boric acid by the electrolysis of sodium borate solutions

6Forward Citations (#16983436 Global)
0.1/yrCitation Velocity (#39203784 Global)
1.93Citation PageRank (#15367472 Global)
3Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

An industrial process is one for the economic production of boric acid and sodium hydroxide or a sodium salt, from sodium borates. Boric acid solution, sodium hydroxide solution, oxygen and hydrogen gases are produced by the electrolysis of sodium borate solutions. Mercury cathode and cation exchange membrane methods have been applied to the electrolysis of sodium borate solutions and, for the economical production of pure boric acid and sodium hydroxide, it was confirmed that the working temperature must be between 60°-100° C., working voltage must be 3.5-5.0 volts, Na 2 O/B 2 O 3 mole ratio at the end of the electrolysis must be 0.15-0.05 and the crystallization temperature must be between 5°-40° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    An economical process for the production of sodium hydroxide and boric acid from borax, including the steps: (a) mixing borax with water to form an aqueous solution of borax; (b) introducing said aqueous solution of borax into an electrolysis cell having cathode and anode compartments; (c) applying a current across said cell to effect electrolysis; (d) maintaining the Na 2 O/B 2 O 3 ratio between about 0.15 and about 0.05 at the anode compartment outlet during electrolysis; (e) collecting sodium hydroxide solution from said cathode compartment; (f) collecting boric acid solution w

  2. Claim 2Depends on #1

    The process as recited in claim 1 which includes the further step of maintaining said aqueous borax solution at a temperature between about 60° C. and 100° C. during electro