Polyethylene terephthalate molding compositions
Abstract
Polyethylene terephthalate molding compositions are provided which comprise a polyethylene terephthalate having an inherent viscosity of at least 0.4, a plasticizer, a lubricating polymer, a nucleating agent, a reinforcing agent or mixture of reinforcing agent and filler, and a molecular weight reducing agent for the polyethylene terephthalate. The molding compositions can be injection molded utilizing mold temperatures below 100° C. (e.g., 60°-90° C.). The molded compositions exhibit an excellent balance of properties such as tensile strength, flex modulus, heat distortion temperature and impact strength.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 21.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Polyethylene terephthalate molding compositions which can be molded at temperatures of 100° C. or less comprising: (a) from about 40 to about 70 parts by weight per 100 parts of total composition of a polyethylene terephthalate having an intrinsic viscosity of 0.4 to 1.0 dl/g as measured at 25° C. in a 1:1: mixture of phenol and tetrachloroethane; (b) from about 0.5 to about 5.0 parts by weight per 100 parts by weight of total composition of a plasticizer selected from the group consisting of benzoate esters of polyols, phthalate esters and phosphate esters; (c) from about 0.5 to about 10.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗