Method of electrodepositing a low coercine force, corrosion-resistant alloy of nickel, iron and boron
Abstract
The present invention deals with alloys consisting essentially of the elements nickel, iron and boron. Boron is present at from 0.1 to 2.0% by weight; iron is present from 17 to 27% by weight and the balance is nickel. The alloy has high resistance to corrosion and H o and H c are less than 0.1 Oe in films 3000Å thick. It is prepared by electrodeposition from a bath having a pH of 2.5 or less, and containing a borane reducing agent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A process for electrodepositing an alloy of high corrosion resistance and H o and H c of less than 0.1 Oe in films 3000 Å thick, said process comprising electrodepositing nickel-iron and boron from an acid bath of pH at or below 2.5 which comprises a borane reducing agent, with the deposited alloy containing approximately 0.1 to 2% by weight boron, from 17% to 27% by weight iron, and the balance nickel.
- Claim 2Depends on #1
A process as claimed in claim 1 wherein the borane reducing agent is dimethylamine borane.
- Claim 3Depends on #1
A process as claimed in claim 1 wherein the bath also contains a pH regulator, a surfactant and sodium saccharin.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (2)
Non-Patent Literature (2)
- W. O. Freitag et al., J. Electrochem. Soc., III, No. 1, pp. 35 39, (Jan. 1964).
- W. O. Freitag et al., J. Electrochem. Soc., III, No. 1, pp. 35-39, (Jan. 1964).