Antistatic thermoplastic molding masses containing styrene-acrylonitrile grafted polyether
Abstract
Thermoplastic molding masses based on the copolymerization of styrene and/or α-methylstyrene and acrylonitrile, which may be modified to be impact resistant with rubberlike polymers, are made antistatic by adding 0.01 to 1.5 percent by weight of a graft polyol which is a polyhydroxy-polyalkylene polyether modified with styrene-acrylonitrile copolymers.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 9.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
An antistatic thermoplastic molding material comprising a copolymer of styrene and/or α-methylstyrene and acrylonitrile and, as an antistatic agent, from 0.01 percent by weight to 1.5 percent by weight of a graft polyol prepared by polymerization of a styrene-acrylonitrile mixture in a polyhydroxy polyalkylene polyether said polyether having a molecular weight of 500 to 10,000 and being obtained by the addition reaction of an alkylene oxide having 2 to 3 carbon atoms with a di- or trifunctional initiator molecule.
- Claim 2Depends on #1
The molding material of claim 1 wherein the antistatic agent is produced by polymerization of a mixture of 5 to 60 percent by weight of styrene/acrylonitrile in a weight ratio of 90:10 to 30:70 and 40 to 95 percent by weight of
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗