Patents
US 4,435,522 A#21082729 Most CitedExpiredUnited States (USPTO)Utility

Method of producing a catalyst for liquefaction of coal

5Forward Citations (#21082729 Global)
0.1/yrCitation Velocity (#42947599 Global)
1.45Citation PageRank (#24161449 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of producing a catalyst for liquefaction of coal comprises heat-treating a salt or oxide of molybdenum or an alloy steel containing at least 0.3 weight percent of molybdenum in the presence of an alkali and water in a carbon monoxide atmosphere at a temperature of 220° to 450° C., and after water rinse and drying, reducing the same in the presence of tetralin and/or a phenol compound in a hydrogen atmosphere at a temperature of 400° to 450° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of producing a catalyst for liquefaction of coal comprising heat-treating a salt or oxide of molybdenum or an alloy steel containing at least 0.3 weight percent of molybdenum in the presence of an alkali and water in a carbon monoxide atmosphere at a temperature of 220° to 450° C., and after water rinse and drying, reducing the same in the presence of tetralin and/or a phenol compound in a hydrogen atmosphere at a temperature of 400° to 450° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗