Process for manufacturing cordierite compositions
Abstract
A process for the manufacture of industrial cordierite ceramic units containing from 45 to 68% by weight of silica 16 to 37% by weight of magnesia and 12 to 45% by weight of alumina which comprises (a) mixing from 15 to 60% by weight of the non-magnetic fraction of asbestos tailings having a MgO:SiO 2 of from 0.8 to 1.25 with 40 to 85% of a kaolin clay by weight and 0 to 10% of alumina; (b) shaping said mixture in green unit forms; (c) curing said units at room temperature for 24 h then at 110° C. for 24 h; (d) firing said cured units at a temperature of from 1350 1400° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for the manufacture of industrial cordierite ceramic units containing from 45 to 68% by weight of silica 16 to 37% by weight of magnesia and 12 to 45% by weight of alumina which comprises (a) mixing from 15 to 60% by weight of the non-magnetic fraction of asbestos tailings having a MgO:SiO 2 ratio of from 0.8 to 1.25 with 40 to 85% of a kaolin clay by weight and 0 to 10% of alumina; (b) shaping said mixture in green unit forms; (c) curing said units at room temperature for 24 h then at 110° C. for 24 h; (d) firing said cured units at a temperature of from 1350°-1400° C.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗