High strength wear resistant aluminium alloys and process
Abstract
Aluminium-silicon alloys of the following composition by weight: ______________________________________ Si 12-15% Cu 1.5-5.5%, preferably 1.5-4% Ni 1.0-3.0% Mg 0.1-1.0% preferably 0.4-1.0% Fe 0.1-1.0% preferably 0.1-0.5% Mn 0.1-0.8% Zr 0.01-0.1% Modifier (preferably Sr) 0.001-0.1% preferably 0.01-0.05% Ti 0.01-0.1% Al Remainder, apart from impurities. ______________________________________ Superior properties are obtained by control of growth rate of the solid phase during solidification and the temperature gradient at the solid-liquid interface. The alloys of the invention are suitable for a wide variety of applications, including brake calipers and drums, piston/bore applications in internal combustion engines and a number of other components in engines, compressors and electric motors. A particular application of the alloys of the invention is in aluminium cylinder heads.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 53.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
An aluminium-silicon alloy consisting essentially of the following composition by weight: ______________________________________ Si 12-15% Cu 1.5-5.5% Ni 1.0-3.0% Mg 0.1-1.0% Fe 0.1-1.0% Mn 0.1-0.8% Zr 0.01-0.1% Silicon modifier 0.001-0.1% Ti 0.01-0.1%
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 53 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,357,450 A | Aluminum alloy | 1944 | 9 |
| US 4,068,645 A | Aluminum-silicon alloys, cylinder blocks and bores, and method of making same | 1978 | 40 |