US 4,433,731 A#1224681 Most CitedExpiredUnited States (USPTO)Utility

Liquid water loss reducing additives for cement slurries

43Forward Citations (#1224681 Global)
1.0/yrCitation Velocity (#6163658 Global)
7.09Citation PageRank (#1873750 Global)
15Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Liquid water loss reducing additives for use in cement slurries are provided comprised of aqueous solutions of low molecular weight carboxymethylhydroxyethylcellulose polymers. Methods of using the additives are also provided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 43.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process for cementing a zone in a well by pumping a cement slurry formed using sea water into said zone and allowing the slurry to harden therein, the improvement comprising the steps of: mixing sea water and a liquid additive for reducing water loss from the slurry during and after placement thereof, said additive being comprised of: water; carboxymethylhydroxyethylcellulose having a carboxymethyl D.S. of about 0.4 and an ethylene oxide M.S. of about 2 and having a molecular weight such that a 5% by weight aqueous solution of said carboxymethylhydroxyethylcellulose at a temperature of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 43 total)

PatentTitleYearCitations
US 7,059,409 B2Methods of cementing and cement compositions containing a polymeric cement cohesion additive20062
EP 0,314,118 A3Cementing composition comprising water-soluble, nonionic hydrophobically modified hydroxyethyl cellulose and its use—0
US 2007105995 A1Fluid loss control additives for foamed cement compositions and associated methods—2
US 7,021,380 B2Compositions comprising set retarder compositions and associated methods200643
US 7,384,894 B2Cement compositions with improved fluid loss characteristics and methods of cementing in surface and subterranean applications20081
WO 9,603,474 A1Drilling fluid additives for improved shale stabilization, the drilling fluid formed therefrom and method of using same—13
US 2006021751 A1Methods of cementing and cement compositions containing a polymeric cement cohesion additive—5
US 2005124503 A1Cement compositions with improved fluid loss characteristics and methods of cementing in surface and subterranean applications—23
US 2004262000 A1Cement compositions with improved fluid loss characteristics and methods of cementing in surface and subterranean applications—40
US 6,405,801 B1Environmentally acceptable well cement fluid loss control additives, compositions and methods200223
US 2004110287 A1Multi-step method for the differentiation of insulin positive, glucose responsive cells—22
US 4,892,589 AComposition comprising water-soluble, nonionic hydrophobically modified hydroxyethyl cellulose and water-soluble, nonionic hydroxyethyl cellulose199025
US 2007137529 A1Cationic cellulose ethers as fluid loss control additives in cement compositions and associated methods—0
US 6,730,636 B2Environmentally acceptable well cement fluid loss control additives, compositions and methods20046
US 5,151,131 ACement fluid loss control additives and methods199287

Non-Patent Literature (1)

  • Oil Well Cementing Practices in the United States, Published by American Petroleum Institute, 1959, pp. 34-37.