Patents
US 4,428,786 A#3573260 Most CitedExpiredUnited States (USPTO)Utility

Process for preparing a high power explosive, high power explosive produced thereby, and method for shaping a high power explosive

22Forward Citations (#3573260 Global)
0.5/yrCitation Velocity (#15013791 Global)
6.52Citation PageRank (#2150194 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A plastic bound high power explosive comprises 90 to 97 percent by weight of a powerful explosive compound, for example octogen, and 3 to 10 percent by weight of a novel stabilizing and binding agent. The agent comprises substantially 20 to 50 percent poly-O-butyl acrylate and 3.5 to 20 percent paraffin, as well as 2 to 7 percent poly tetrafluorethylene as a lubricant, 20 to 65 percent of a filler and 1 to 8 percent poly ethylene or, respectively, in the case of an antistatic high power explosive, 25 to 65 percent graphite as a lubricant and 15 to 25 percent calcium sulphate as a filler, each by weight of the portion of solids in the agent. Further additives like emulsifiers, dispersants, defoamers, surfactants, thickeners and small amounts of silica gel are added. The stabilizing and binding agent is prepared as an aqueous dispersion which is mixed with the dry explosive compound in a mixing drum, then dried or, respectively, predried and treated with an isopropanol-water mixture (1:1) prior to being finally dried. Homogeneous bodies cold-pressed therefrom using a die at pressures in the range of about 1.5 to 4.2 kbar/cm 2 have densities above 1.8 g/cm 3 and their detonation veloc

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 22.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a high power explosive, said process comprising the steps of: preparing an aqueous dispersion of a stabilizing and binding agent by mixing an aqueous polymer dispersion with a lubricant, with an aqueous paraffin dispersion and with a filler in the presence of usual additives; blending said aqueous dispersion of said stabilizing and binding agent with a dry powerful explosive compound selected from the group consisting of cyclotetramethylenetetranitramine and cyclotrimethylenetrinitramine; and warm-drying the blend thus obtained to yield a high power explosive compri

  2. Claim 2Depends on #1

    Process as in claim 1 wherein the aqueous polymer dispersion is prepared from poly-O-alkyl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Chemical Abstracts, vol. 90, p. 121, 74067j, 1979; Chugoku Kayaku Co. Ltd.