Patents
US 4,427,490 A#584839 Most CitedExpiredUnited States (USPTO)Utility

Delignification and bleaching process for lignocellulosic pulp with peroxide in the presence of metal additives

64Forward Citations (#584839 Global)
1.5/yrCitation Velocity (#3372151 Global)
9.10Citation PageRank (#1239717 Global)
18Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process and solution for delignifying and brightening lignocellulosic pulp. The solution comprises from about 0.1 to about 5% by weight, based on oven-dried pulp of a peroxide and about 0.5 to about 20 mole percent, based on the moles of peroxide, of a metal ion selected from the group consisting of tungsten, molybdenum, chromium, osmium and selenium. The preferred process of this invention comprises contacting a lignocellulosic pulp with about 0.5 to about 20 mole percent, based on moles of peroxide, of a metal ion selected from the group consisting of tungsten, molybdenum, chromium, osmium and selenium at a temperature below about 50° C.; adjusting the pH of the resultant pulp slurry to between about 1 and about 7; adding 0.1 to about 5% by weight based on oven-dried pulp of peroxide and effecting pulp delignification and brightening at about 30° C. to about 100° C. until most of the peroxide has been consumed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 64.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for delignifying and brightening lignocellulosic pulp comprising maintaining the temperature of an aqueous hydrogen peroxide-containing pulp slurry between about 30° C. and 100° C. until the peroxide is substantially consumed, the pulp slurry comprising lignocellulosic pulp; from about 0.1 to about 5% by weight, based on oven-dried pulp, of hydrogen peroxide and about 0.5 to about 20 mole percent, based based on moles of the peroxide, of tungsten ion; and having a pH between about 3 and about 6; the peroxide and the tungsten ion, as present in the pulp slurry, consisting essentially

  2. Claim 2Depends on #1

    The process of claim 1 wherein the pH is 5 and the slurry temperature is 77° C.

  3. Claim 3Independent Claim

    A process for delignifying and brightening lignocellulosic pulp comprising admix

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 64 total)

PatentTitleYearCitations
US 2024263394 A1Modified sulfuric acid and uses thereof—2
US 9,909,257 B2Modified cellulose from chemical kraft fiber and methods of making and using the same20183
US 9,512,563 B2Surface treated modified cellulose from chemical kraft fiber and methods of making and using same20164
US 7,297,225 B2Process for high temperature peroxide bleaching of pulp with cool discharge20072
US 6,432,266 B1Process for bleaching chemical pulp simultaneously with chlorine dioxide, peroxide and a reaction catalyst200222
DE 102008040884 A1Recovering e.g. molybdate from aqueous solution comprises contacting the solution with cationized inorganic carrier material, separating carrier material from the solution, contacting carrier material with aqueous solution and separating—3
US 11,111,628 B2Modified cellulose from chemical kraft fiber and methods of making and using the same20210
US 2009274598 A1Process for Recovering Molybdate or Tungstate from Aqueous Solutions—7
US 8,545,673 B2Process for recovering molybdate or tungstate from aqueous solutions201316
US 2005098279 A1Method for bleaching mechanically defibered pulp—0
US 9,777,432 B2Modified cellulose from chemical kraft fiber and methods of making and using the same20173
US 8,277,765 B2Process for recovering molybdate or tungstate from aqueous solutions20125
US 8,262,850 B2Chemical activation and refining of southern pine kraft fibers20122
US 9,926,666 B2Modified cellulose from chemical kraft fiber and methods of making and using the same20182
US 9,512,562 B2Modified cellulose from chemical kraft fiber and methods of making and using the same20163

Non-Patent Literature (5)

  • Christensen; "Bleaching of Sulphate Pulps with Hydrogen Peroxide", Norsk Skogindustri, pp. 268-271.
  • Holladay et al., "The Bleaching of Pulp" Chapt. 9, 180-185, Mack Printing Co. 1963.
  • McCloskey et al.; "Catalytic Influence of Iron and Magnesium Ions in O2 Bleaching Reactions" TAPPI; vol. 58, No. 2 2-1975.
  • Rapson; "The Role of pH in Bleaching Pulp", TAPPI pp. 284-294, vol. 39, No. 5.
  • Schurb et al.; Hydrogen Peroxide, pp. 658-661.