GaAs FETs Having long-term stability
Abstract
GaAs FETs exhibit excellent long-term stability if they have a drain ledge, a drain contact with reduced dendrite size, and a silicon nitride passivation layer. Accelerated aging tests at device case temperatures of 250 degrees C. indicate essentially no device failures after 200 hours of observation and a median failure time of approximately 500 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a field effect transistor device comprising an active region of GaAs, a source, a gate, and a drain wherein said drain comprises a drain ledge contacting said active region and an electrical contact to said drain ledge CHARACTERIZED IN THAT said device is passivated with a material that prevents oxidation of said active region, said ledge extends beyond the edge of said contact in the direction of said gate, and dendrites formed during the fabrication of said contact terminate with the boundaries of said ledge.
- Claim 2Depends on #1
The device of either claim 1 wherein the extension of said ledge beyond said contact is at least equal to the thickness of said active region at a point below said gate.
- Claim 3Depends on #1
The device of either claim 1 wherein said passivating material comprises silicon nitride.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 4,196,439 A | Semiconductor device drain contact configuration | 1980 | 17 |
| US 4,301,188 A | Process for producing contact to GaAs active region | 1981 | 20 |