Method for the production of more water-resistant foamed elements from waterglass containing natural latex dispersion
Abstract
A method for the production of a more water-resistant foamed element from waterglass consisting essentially of the steps of mixing together a major amount of an alkali metal silicate solution, with inorganic fillers, at least one alkali-resistant wetting agent in an amount sufficient to form a stable foam, at least one compound capable of hardening a waterglass foam in an amount sufficient to cause said alkali metal silicate to harden, and sufficient natural latex dispersion to cause the foamed element to have a greater water resistance, mechanically foaming said mixture by the incorporation of an inert gas thereon, filling the resultant foam into an element form capable of disassembly, curing said foam in said form, and recovering a more water-resistant foamed and cured element. Preferably the natural latex dispersion is employed in a 50% dispersion in an amount of from 0.2% to 30% by weight, preferably from 0.2% to 10% by weight, based on the total mixture. The alkali metal silicate solution used has, in the case of sodium silicate, a solids content of about 27% to 43% by weight at an SiO 2 /Na 2 O molar ratio of about 4 : 1 to 3 : 1 and in the case of potassium silicate a solids
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 12.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for the production of a more water-resistant foamed element from waterglass consisting essentially of the steps of mixing together a major amount of an alkali metal silicate solution, with inorganic fillers, at least one alkali-resistant wetting agent in an amount sufficient to form a stable foam, at least one compound capable of hardening a waterglass foam in an amount sufficient to cause said alkali metal silicate to harden, and sufficient natural latex dispersion to cause the foamed element to have a greater water resistance, mechanically foaming said mixture by the incorporation o
- Claim 2Depends on #1
The method of claim 1 wherein a 50% aqueous natural latex dispersion is used in an amount of from 0.2% to 30%
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- Chemical Abstracts, "Moldings of Foamed Water Glass" Karl Weber-8/6/70-(corres. to 1905340).