Patents
US 4,415,380 A#49661801 Most CitedExpiredUnited States (USPTO)Utility

Method for making a high remanence Fe-Mo-Ni magnetic element

1Forward Citations (#49661801 Global)
0.0/yrCitation Velocity (#60284872 Global)
0.88Citation PageRank (#49100216 Global)
7Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Magnetically actuated devices such as, e.g., switches and synchronizers typically comprise a magnetically semihard component having a square B-H hysteresis loop and high remanent induction. Among alloys having such properties are Co-Fe-V, Co-Fe-Nb, and Co-Fe-Ni-Al-Ti alloys which, however, contain undesirably large amounts of cobalt. According to the invention, devices are equipped with a magnetically semihard, high-remanence Fe-Mo-Ni alloy which comprises Mo in a preferred amount in the range of 2-26 weight percent and Ni in a preferred amount in the range of 0.5-15 weight percent. Magnets made from alloys of the invention may be shaped, e.g., by cold drawing, rolling, bending, or flattening and may be used in devices such as, e.g., electrical contact switches, hysteresis motors, and other magnetically actuated devices. Preparation of alloys of the invention may be by a treatment of annealing and aging or deformation and aging.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Method for making a magnetic element consisting of a body of a metallic alloy having a magnetic squareness ratio which is greater than or equal to 0.9 and having remanent magnetic induction which is greater than or equal to 13000 gauss, said alloy comprising an amount of at least 99.5 weight percent Fe, Mo, and Ni, Mo being in the range of 2-26 weight percent of said amount and Ni being in the range of 0.5-15 weight percent of said amount, said method comprising the steps of (1) annealing said body by heating at a temperature in a range of 900-1200 degrees C., (2) rapidly cooling the annealed

  2. Claim 2Depends on #1

    Method of claim 1 in which aging is for a time in the range of 5 minutes to 10 hours.

  3. Claim 3Independent Claim

    Method of cl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

Non-Patent Literature (5)

  • H. Masumoto, "Characteristics of Fe-Mo and Fe-W Semihard Magnet Alloys", Journal of the Japanese Institute of Metals, vol. 43, 1979, pp. 506-512.
  • K. S. Seljesater et al., "Magnetic and Mechanical Hardness of Dispersion Hardened Iron Alloys", Transactions of the American Society for Steel Treating, vol. 19, pp. 553-576.
  • L. R. Moskowitz, Permanent Magnet Design and Application Handbook, Cahners Books, 1976, pp. 211-220.
  • M. R. Pinnel, "Magnetic Materials for Dry Reed Contacts", IEEE Transactions on Magnetics, vol. MAG-12, 1976, pp. 789-794.
  • Metals Handbook, 8th Ed., vol. 8, American Society for Metals, 1973, p. 431.