Patents
US 4,412,937 A#2782550 Most CitedExpiredUnited States (USPTO)Utility

Method for manufacture of activated carbon fiber

26Forward Citations (#2782550 Global)
0.6/yrCitation Velocity (#12961464 Global)
7.36Citation PageRank (#1762557 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for manufacturing activated carbon fibers is disclosed. The method is comprised of the steps of: (1) causing an acrylic fiber to contain therein a treating agent selected from the group consisting of phosphorus and boron compounds in a concentration of 0.01 to 0.3% by weight as phosphorus or boron based on the weight of the fiber; (2) preoxidizing the acrylic fiber in an oxidizing atmosphere at a temperature exceeding 200° C. and giving a core ratio of 18% until the amount of bonded oxygen becomes not less than 15% by weight based on the weight of the fiber thereby producing a preoxidized fiber; (3) adjusting the concentration of the treating agent in the preoxidized fiber to a level in the range of 0.04 to 1% by weight based on the thus obtained preoxidized fiber; and (4) thereafter activating the fiber at a temperature in the range of 900° to 1,300° C. The resulting fiber has improved high strength, high adsorbing ability and high processibility.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 26.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing acitivated carbon fiber, comprising the steps of: (1) causing an acrylic fiber to contain therein a treating agent, wherein the treating agent is selected from the group consisting of phosphorus and boron compounds in a concentration of 0.01 to 0.3% by weight as phosphorus, boron, or a mixture thereof, based on the weight of the fiber; (2) preoxidizing the acrylic fiber in an oxidizing atmosphere at a temperature exceeding 200° C. and giving a core ratio of not more than 18% until the amount of bonded oxygen becomes not less than 15% by weight based on the weight o

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗