Method of making a dispersion lacquer for luminescent screens
Abstract
After being deposited on the luminescent screen, the dispersion lacquer made by the method disclosed forms a smooth and uniform film whose fluidity can be influenced. This results in an improved reflectance behavior of the deposited aluminum film and, thus, in greater picture brightness. The disclosed method consists in that a boric-acid solution is added to the dispersion lacquer which is then set to the desired viscosity by means of a neutralizer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 4.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
Method of making a dispersion lacquer containing a boric-acid compound and intended for use as a volatilizable substrate layer during the metallization of a luminescent screen, wherein an aqueous emission of a polyacrylate, an inorganic binder, and an oxidizing agent are used, the improvement comprising the steps of: adding an aqueous solution of a polyvinylalcohol and a boric-acid solution as separate ingredients at approximately room temperature; and adding a neutralizer to adjust the pH value of the dispersion lacquer to a desired level, whereby a desired viscosity is obtained.
- Claim 2Depends on #1
A method as claimed in claim 1, wherein a 0.1-5 weight percent boric-acid solution is added to the dispersion.
- Claim 3Depends on #1
A method as claimed in claim 1, wherein 0.1 to 10 percent by weight of boric acid referred to the content of solid acrylate
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗