Use of rod mill for initial stage of solder glass grinding
Abstract
A dramatic reduction in the time required to fine-grind high borate solder glasses is achieved. In the prior art method, the glass is ball-milled in the presence of an amine for about seven days or more. It has now been discovered that by first rod-milling such glasses for a period of from about 1/2 to about 24 hours, the time required for the "amine grind" can be shortened to a period of from about 1 to 3 days. A further improvement is that rod milling eliminates the laborious sieving procedure previously employed to ensure the absence of undesirably large particles in the feed to the amine grinding operation.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
The method of grinding an alkali metal borate glass which comprises: a. charging to a rod mill particles of said glass comprising from about 60 to about 97 mole percent of B 2 O 3 and a total of from about 3 to about 30 mole percent of one or more alkali metal oxides, said glass having a Vickers hardness number of from about 200 to about 700, said rods and the mill lining having Vickers numbers higher than that of the glass and being composed of the same or different, non-brittle materials; b. grinding said glass in said mill until the particles have a volume average diameter greater
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (8)
Non-Patent Literature (1)
- "Action in a Rod Mill", Engineering & Mining Journal, vol. 161, No. 3, pp. 82-85.