Process for the preparation of thermoplastic aromatic polyphosphonatocarbonates with improved heat-ageing resistance, and their use
Abstract
Thermoplastic polyphosphonatocarbonates prepared by polycondensing at least one aromatic dihydroxy compound with a diaryl carbonate and a phosphonic acid diaryl ester in the presence of a catalyst selected from the group consisting of (a) tetra-C 1 -C 18 -alkyl titanates, (b) di-C 2 -C 4 -alkyl-tin oxides, (c) di-C 2 -C 4 -alkyl-di-C 1 -C 4 -alkoxy-tin compounds, (d) tetra-C 3 -C 18 -alkyl zirconates, (e) tri-C 2 -C 18 -alkyl vanadylates and (f) mixtures of germanium dioxide or titanium dioxide and at least one of (a) to (e) in a weight ratio of 1:3 to 3:1 at a temperature of from 80°-340° C. and under a pressure of 600 to 0.1 mm Hg in an inert gaseous atmosphere, the molar ratio of diaryl carbonate to phosphonic diaryl ester being from 5:95 to 95:5 and the molar ratio of aromatic dihydroxy compound to the sum of diaryl carbonates and phosphonic diaryl ester being from 0.91:1 to 0.99:1.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 33.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for preparing an aromatic, thermoplastic polyphosphonatocarbonate of improved heat-ageing resistance which comprises polycondensing (A) at least one aromatic dihydroxy compound having 6 to 30 carbon atoms with (B) a diaryl carbonate having 6 to 14 carbon atoms in each aryl moiety and (C) a phosphonic acid diaryl ester having 6 to 14 carbon atoms in each aryl moiety in the presence of 10 -7 to 2.10 -2 mole percent, per mole of aromatic dihydroxy compound, of at least one catalyst selected from the group consisting of (a) tetra-C 1 -C 18 -alkyl titanates, (b) di-C 2 -C 4 -alkyl-t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗