Process for cobalt recovery from mixed sulfides
Abstract
The metal content of nickel-cobalt mixed sulfide slurries is recovered by atmospheric oxidation leaching, thereafter removing dissolved copper by metathesis with further mixed sulfide feed, treating the filtrate after liquid-solids separation with ammonia to selectively precipitate cobalt, separating the cobalt precipitate and working up the resulting filtrate to recover nickel.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 13.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process resulting in the preferential recovery of cobalt occurring from the separation of cobalt, nickel, and copper values contained in a precipitated cobalt, nickel and copper sulfide feed material, the process comprising: (a) slurrying the sulfide material in an aqueous medium essentially free of sulfuric acid to provide a slurry containing about 5% to about 30% solids by weight, the slurry not exceeding 10 grams of ammonia per liter, the pH of the slurry ranging from about 5 to 8 pH units, (b) oxidatively leaching the slurry at atmospheric pressure by aerating the slurry with an oxygen
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (13 of 13 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (2)
- "Llanos, Z. R. Atmospheric Leaching of Matte at Port Nickel Refinery" Hydrometallurgy, Oct. 1973, p. 74.
- Plasket, R. P., Recovery of Nickel and Copper from High Grade Matte at Impala Platinum by The Sherritt Process, AIME-TMS A74-102.