Patents
US 4,397,696 A#10282297 Most CitedExpiredUnited States (USPTO)Utility

Method for producing improved aluminum conductor from direct chill cast ingot

10Forward Citations (#10282297 Global)
0.2/yrCitation Velocity (#30671888 Global)
2.29Citation PageRank (#11690117 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Aluminum conductor is made from direct chill cast (DC) ingot with improved conductivity and creep resistance by heating an aluminum-base alloy ingot containing not more than 0.40 wt. % and preferably not more than 0.30 wt. % Fe or a mixture of Mg, Ni or Zr with Fe to a temperature of 400 DEG to 600 DEG C., hot rolling the ingot in this temperature range and then further hot rolling at a reduced temperature range of 175 DEG to 325 DEG C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 10.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for the production of an aluminum conductor having improved creep resistance from an aluminum-base alloy ingot containing up to 0.40 wt.% of one of the group consisting of Fe, Mg, Ni, Cu, Si and Zr and not more than 0.9 wt.% when more than one of these elements are present and cast by the direct chill casting process which comprises: (a) heating the aluminum-base alloy ingot to a temperature of from about 400° to 640° C. and maintaining the ingot at this temperature for from 1/2 to 10 hours; (b) hot rolling the ingot at a first temperature of 400° to 600° C.; and (c) hot rolling t

  2. Claim 2Depends on #1

    The method of claim 1 wherein the iron content is not more than 0.40 wt.%.

  3. Claim 3Depends on #1

    The method of claim 1 wherein the iron content is from 0.02 to 0.30 wt.%.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗