Process for the production of a hard solid solution containing molybdenum
Abstract
The present invention relates to a process for the production of a solid solution constructed of at least one hard phase having a crystal structure of simple hexagonal type and selected from mixed carbides or carbonitrides of molybdenum and tungsten, which process comprises preparing an alloy powder consisting of a solid solution of molybdenum and tungsten, adding to the alloy powder carbon in an amount necessary for forming (Mo, W)2C and/or (Mo, W)2(CN), heating the mixture at a temperature at which (Mo, W)2C and/or (Mo, W)2(CN) is stable, adding to the (Mo, W)2C and/or (Mo, W)2(CN) carbon in an amount necessary for forming (Mo, W)C and/or (Mo, W)(CN) optionally with an iron group metal and then heating the mixture at a temperature at which (Mo, W)C and/or (Mo, W)(CN) is stable.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the production of a hard solid solution comprising at least one hard phase having a crystal structure of simple hexagonal type and being represented by (Mo a W b )C z or (Mo a W b )(CN) z wherein z=0.9 to 1.0 and a+b=1, which process comprises: (a) preparing an alloy powder consisting of a solid solution of molybdenum and tungsten and adding to the alloy powder carbon in an amount sufficient to give a mixture wherein z=0.4 to 0.6, (b) heating the mixture at a temperature of at least 1400° C., and in an atmosphere containing nitrogen in the case of forming the carbonitride,
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗