Patents
US 4,384,098 A#7179311 Most CitedExpiredUnited States (USPTO)Utility

Filamentary polypropylene and method of making

13Forward Citations (#7179311 Global)
0.3/yrCitation Velocity (#25393914 Global)
8.37Citation PageRank (#1426120 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In accordance with the present invention, novel lustrous, filamentary polypropylene products are produced by melt spinning a polypropylene resin, having a molecular weight distribution of less than about 7 and a melt flow between about 20 and about 60, at a spinning temperature below about 510° F. and taking up the spun filaments at a speed above about 1200 meters per minute. A novel product having a high degree of luster is also produced in accordance with the present invention.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for making filamentary materials having a high degree of lustre, comprising: melt spinning a polypropylene resin, having a molecular weight distribution of less than about 7 and a melt flow between about 20 and about 60, at a spinning temperature below about 510° F. and at a takeup speed above about 1000 meters per minute.

  2. Claim 2Depends on #1

    A process in accordance with claim 1 wherein the spinning temperature is between about 420° and about 480° F.

  3. Claim 3Depends on #2

    A process in accordance with claim 2 wherein the spinning temperature is about 460° F.

Technical Overview & Description