Austenite alloy tubes having excellent high temperature vapor oxidation resistant property

13Forward Citations (#7321184 Global)
0.3/yrCitation Velocity (#25418008 Global)
3.54Citation PageRank (#5800731 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The austenite alloy tube has a composition of 15 DIFFERENCE 26% of Cr, 8 DIFFERENCE 35% of Ni, 1.0% or less of Si, 2.0% or less of Mn and less than 0.25% of N and the balance of iron and impurities. The nitrogen content on the inner surface of the tube is at least 0.25%. If desired, one or more of 0.6% or less of Ti, 0.6% or less of Al, 3.0% or less of Mo and 1.0% or less of Nb may be incorporated.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 13.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    An austenite alloy tube having excellent high temperature steam oxidation resistant properties having a composition comprising 15 to 26% by weight of chromium, 8 to 35% nickel, silicon in an amount up to 1%, manganese in an amount up to 2%, said tube having an average nitrogen content of less than 0.25%, and having a nitrogen content of 0.25% or higher on the inner surface of said tube, said inner surface having been nitrided to provide said higher nitrogen content, and the balance of said tube being iron and impurities.

  2. Claim 2Depends on #1

    The austenite alloy tube of claim 1 wherein said composition further comprises at least one of titanium in an amount up to 0.6%, aluminum in an amount up to 0.6%, molybdenum in an amount up to 3%, and niobium in an amount up to 1%.

  3. Claim 3Depends on #1

    The austenite alloy tube of claim 1 wherein said tube has