Patents
US 4,381,271 A#4153581 Most CitedExpiredUnited States (USPTO)Utility

Use of fired fibrous graphite in fabricating polycrystalline diamond and/or cubic boron nitride/silicon carbide/silicon composite bodies

20Forward Citations (#4153581 Global)
0.5/yrCitation Velocity (#17467218 Global)
4.32Citation PageRank (#4198055 Global)
6Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Disclosed is an improvement in a process for fabricating a polycrystalline diamond and/or cubic boron nitride-silicon carbide-silicon composite body fabricated by infiltrating silicon through a mixture of a carbonaceous material and non-diamond carbon coated diamond and/or cubic boron nitride under partial vacuum at elevated temperature. Such improvement comprises providing fibrous graphite for inclusion in the mixture, said fibrous graphite being subjected to heat treatment at a temperature of between about 800° and 1700° C. prior to its inclusion in the mixture and at a temperature of between about 800° and 1550° C. after its inclusion in the mixture. Such heat treatment is conducted under a total pressure of less than about 1 Torr. The vacuum silicon infiltration then is practiced on the mixture which includes the heat treated graphite fibers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 20.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In a process for making a shaped polycrystalline body having a volume greater than 10 cubic millimeters comprised of a mass of crystals selected from diamond, cubic boron nitride, and combinations thereof adherently bonded together by a bonding medium of silicon carbide and elemental silicon, said crystals comprising between 1 and 70 volume percent of said body, which process comprises: (a) infiltrating a substantially uniform mixture of said crystals and fibrous graphite with fluid silicon under a partial vacuum at a temperature above 1400° C.; and (b) cooling and recovering the infiltrated

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗