Raw polymer powder of a modified tetrafluoroethylene polymer having a high bulk density and a good powder flow index and also a process for the manufacture and use thereof

2Forward Citations (#2773 Global)
0.1/yrCitation Velocity (#45608 Global)
3.58Citation PageRank (#2257 Global)
8Prior Art Cited
2Structured Claims
0Drawings / Sheets

Abstract

Novel granular, free-flowing, non-melt-fabricable raw polymer powders of tetrafluoroethylene polymers consisting of 0.004 to 0.075 mole % of polymerized units of a perfluoroalkyl vinyl ether and of tetrafluoroethylene units, are described. These powders have an average particle diameter of 450 to 1,400 μm, a bulk density of at least 570 g/l, a powder flow index of ≦5 seconds/50 g and a grain stability of ≦5.5 seconds/50 g. They are prepared direct by suspension polymerizing TFE in the presence of the perfluoroalkyl ether, while stirring, the calculated concentration of the ether in the gas phase being kept within the range from 0.1 to 1.0% by volume in the period of time until 1.5% by weight of solid polymer have been formed, and the polymerization being carried out under a total pressure of 5 to 11 bars. A further improvement in bulk density, powder flow and grain stability is achieved if the intensity of stirring is kept at a relatively low level in a critical range, beginning at the formation of 1.5 to 3% by weight of solid polymer and extending to the formation of 8 to 12% by weight of solid polymer. The raw polymer powders which can be obtained in this manner are suitable, as

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 2.

Claims (2)

  1. Claim 1Independent Claim

    In a granular, free-flowing, non-melt-fabricable, non-presintered raw polymer powder of a tetrafluoroethylene polymer, consisting essentially of from 0.004 to 0.075 mole percent polymerized units of a perfluoroalkyl vinyl ether of the formula CF.sub.2 ═CF--O--R.sub.f wherein R f is C 2 F 5 , n-C 3 F 7 , or n-C 4 F 9 , and of polymerized tetrafluoroethylene units having a specific surface of from 0.5 to 4.5 m 2 /g, the improvement residing in the fact that said powder has an average particle diameter d 50 of from 450 to 1400 μm, a bulk density of at least 570 g/l, a powder flow inde

  2. Claim 2Depends on #1

    A raw polymer powder of a tetrafluoroethylene polymer as claimed in claim 1 having a bulk density of from 620 to 750 g/l. 3