US 4,374,012 A#14135865 Most CitedExpiredUnited States (USPTO)Utility

Method of making semiconductor device having improved Schottky-barrier junction

7Forward Citations (#14135865 Global)
0.2/yrCitation Velocity (#37821811 Global)
4.20Citation PageRank (#4393016 Global)
16Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A semiconductor device having an improved non-diffusive Schottky-barrier junction and metallization layers and method for producing the same. A thin layer of a Schottky-barrier forming metal such as platinum is sputter deposited upon a hot gallium arsenide substrate, thereby impact alloying a portion of the Schottky-barrier forming metal with the gallium arsenide material. A refractive metal such as titanium is then sputtered above the Schottky-barrier forming layer at a power level sufficient to alloy the remaining Schottky-barrier forming metal with the refractive metal. A highly conductive layer such as gold is then sputter deposited over the refractive layer to provide ohmic contact. The invention may be used to particular advantage in microwave diode and field effect transistor devices.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 7.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The method comprising the steps of: providing a body of semiconductor material; sputtering a Schottky-barrier forming metal upon at least a portion of a surface of said body of semiconductor material at a sputtering power level sufficient to cause alloying between a portion of said semiconductor material and at least a portion of the sputtered Schottky-barrier forming metal; sputtering a layer of refractory metal over said sputtered Schottky-barrier forming metal; and sputtering a layer of highly conductive metal over said layer of refractory metal.

  2. Claim 2Depends on #1

    The method of claim 1 further comprising the step of: heating said body of semiconductor material to a temperature in the range of 300° to 350° C. prior to sputtering said Schottky-barrier forming metal.

  3. Claim 3Depends on #1

    The method of claim 1 wherein said step of sput

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Electronics Letters, vol. 11, No. 18, Sep. 4, 1975, High Power C Band Impatt Diodes, pp. 430-431.