Mineral wool and process for producing same
Abstract
A process for producing mineral wool having a chemical composition comprised of between about 50 and 70 weight percent silica plus alumina, about 20 and 35 weight percent lime plug magnesia and about 5 and 15 weight percent iron oxides is described. The process includes feeding a first particulate waste material having a particle size of 100 weight percent -200 mesh and containing organic combustibles having heating values of about 10 mega J per kilogram of slag and inorganic non-combustibles, a second particulate waste material having a particle size of 100 weight percent -200 mesh and containing fluxstone, and preheated air at a velocity of between about 30 meters to 60 meters per second at a temperature of about 500° C. into a high temperature cyclone-like furnace. The combustibles are substantially instantaneously burned and the non-combustibles and the fluxstone are melted and reacted to form a molten slag which can be fiberized into mineral wool.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 44.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing mineral wool wherein a molten slag substantially free of metallic iron and suitable for fiberizing into mineral wool is formed in a cyclone-type furnace having a combustion zone, a collecting zone and an exhaust gases-combustion air heat exchanger, the process comprising: (a) feeding (i) a first particulate material containing organic combustibles and inorganic non-combustibles and characterized by a composition comprised of between: about 49-62 weight percent silica, about 21-27 weight percent alumina, about 1.0-3.0 weight percent lime, about 0.5-3.0 weight percent mag
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗