Tin-base body solder
Abstract
In a preferred embodiment, a method is presented for filling depressions in fabricated steel surfaces by applying a metallic body solder consisting of 14 to 20 weight percent copper, 1 to 7.5 weight percent zinc, 0.5 to 1.5 weight percent iron and the balance tin. The body solder alloy is heated to form workable thixotropic paste that is applied with spreading onto the steel surface. Upon cooling, the body solder forms a dense, tightly adherent fill that is grindable and paintable in conjunction with the surrounding steel surface.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 18.
Claims (3 — 3 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for filling a depression in a fabricated metal surface by applying to said surface a workable thixotropic paste formed by heating an alloy comprising about 10 to 25 weight percent copper, 0.25 to 1.5 weight percent iron, zero to 7.5 weight percent zinc and the balance tin.
- Claim 2Independent Claim
A method for filling a depression in a fabricated steel surface by applying to said surface a workable thixotropic paste formed by heating to a temperature above about 210° C. an alloy comprising about 14 to 20 weight percent copper, 0.5 to 1.5 weight percent iron, about 1 to 7.5 weight percent zinc and the balance tin.
- Claim 3Independent Claim
A method for filling a depression in a fabricated steel surface, said method comprising casting a tin-base alloy consist
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗