Method for recovery of terephthalic acid from polyester scrap
Abstract
Polyester scrap such as film (plain or silver-bearing), fabric, yarn or bottles, based primarily on polyethylene terephthalate, is depolymerized at room temperature and atmospheric pressure with a mixture of concentrated sulfuric acid and water to form crude terephthalic acid which is purified by dissolving in alkali solution, filtering to remove impurities, acidifying the filtrate to recover terephthalic acid in high yield with a purity of at least 99%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 70.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for the recovery of purified terephthalic acid from terephthalate polyester scrap substantially free of metals, said method comprising the steps of: (a) dissolving the polyester in a mixture of sulfuric acid and water in a volume ratio of 8.5-13 to 2 for a period of up to 30 minutes to form a precipitate of crude terephthalic acid; (b) diluting the reaction mixture from step (a) with at least an equal volume of water and separating the crude terephthalic acid; (c) treating the crude terephthalic acid from step (b) with water and a base selected from the group consisting of potassi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 70 total)
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CA 523,222 A | Recovery of dicarboxylic acids from polyesters | 1956 | 1 |