Patents
US 4,339,282 A#635889 Most CitedExpiredUnited States (USPTO)Utility

Method and composition for removing aluminide coatings from nickel superalloys

61Forward Citations (#635889 Global)
1.4/yrCitation Velocity (#4005968 Global)
14.44Citation PageRank (#576105 Global)
7Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Nickel aluminide and like coatings are stripped from nickel base superalloy substrates using a 60°-71° C. solution consisting essentially by volume percent of 43-48 nitric acid, 7-12 hydrochloric acid, balance water, and containing 0.008-0.025 mole/liter ferric chloride and at least 0.016 mole/liter copper sulfate. Coating removal is rapid while significant attack of the substrate is avoided.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 61.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    The process of removing an aluminide coating from a nickel superalloy article characterized by contacting the coating with a stripping solution having a composition consisting essentially by volume percent of 43-48 concentrated nitric acid, 7-12 concentrated hydrochloric acid, 40-50 water, at least 0.016 mole/liter CuSO 4 and 0.008-0.025 mole/liter ferric chloride.

  2. Claim 2Depends on #1

    The process of claim 1 wherein the composition is more particularly characterized as 43-48 concentrated nitric acid and 9-11 concentrated hydrochloric acid, 41-48 water, and wherein the molar ratio of FeCl 3 and CuSO 4 is maintained at about 1:2.

  3. Claim 3Depends on #1, #2

    The process of claims 1 or 2 wherein the solution is maintained at about 60°-71° C. and wherein the article is removed from contact with the solution and vapor blasted at periodic intervals.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗