Abstract

A method for making a selective absorption film for solar energy which comprises immersing aluminum or its alloy in water which contains at least two members selected from phosphate ions, fluoride ions and triethanolamine, and optionally ions of a metal selected from copper, iron, cobalt, silver and a mixture thereof thereby forming a chemical conversion film which shows a great absorptivity and a small emissivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 21.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for the production of a selective absorption film for solar energy which comprises immersing aluminium or its alloy in water solution which consists essentially of at least two members selected from the group consisting of phosphate ions, fluoride ions and triethanolamine for a sufficient time to form a chemical conversion film on the aluninium or its alloy, wherein said immersion is conducted at a temperature not lower than 80° C. for a time of at least 10 minutes, the concentration of the phosphate ions or the fluoride ions is in the range of 20-300 ppm, and the concentration of tri

  2. Claim 2Depends on #1

    A method according to claim 1, wherein the water contains phosphate and fluoride ions and triethanolamine.

  3. Claim 3Depends on #1

    A method according to claim 1, further comprising ions of a metal s