Method for recovering residual matter accumulated in the production and machining of steel
Abstract
A method of recovering particulate matter having a high metal content and including dust resulting from production of steel and chips from machining of steel. The method includes selecting the chips that have a length of 7 to 30 mm; mixing the dust and the selected chips in the ratio of about 70:20 to 30:60 pts/pts; wetting the dust, before or after it has been mixed with the chips, to a moisture content of 3 to 8% by weight to hydrate free lime in the dust; and mixing the dust and selected metal chips with a suitable binder; and forming the mixture into briquettes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method in which residual matter of the type accumulated as metal-containing dust and chips in the production and machining of steel is to be formed into briquettes, with the addition of a binder, the steps comprising: selecting the chips to have a length of about 7 to 30 mm; 3% to 8% by weight of water; allowing the moistened dust time to hydrate free lime contained in the dust; and forming a mixture of the dust, binder, and chips into briquettes.
- Claim 2Depends on #1
The method according to claim 1 in which the water is in the form of steam.
- Claim 3Depends on #1
The method according to claim 1 in which the water is added to metal-containing dust to make the weight of the water content thereof 4% to 7% of the weight of the dust.