Patents
US 4,335,216 A#2467017 Most CitedExpiredUnited States (USPTO)Utility

Low temperature fired dielectric ceramic composition and method of making same

28Forward Citations (#2467017 Global)
0.6/yrCitation Velocity (#12250130 Global)
12.05Citation PageRank (#778727 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Low temperature fired dielectric ceramic compositions are prepared by firing, at temperatures between about 1000° C. and about 1150° C., a base ceramic preparation comprising barium titanate, strontium titanate, barium zirconate, titanium dioxide and manganese dioxide mixed with a glass frit comprising zinc oxide, silicon dioxide, boron oxide, lead oxide, bismuth tioxide, and cadmium oxide. The resulting dielectric ceramic composition is useful to form multilayer ceramic capacitors.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 28.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A dielectric ceramic composition formed from about 92 to about 96.5 percent by weight of a base ceramic preparation which base ceramic preparation consists essentially of from about 72 to about 80 weight percent barium titanate, from about 6 to about 15 weight percent strontium titanate, from about 6 to about 15 weight percent barium zirconate, from about 0.4 to about 0.8 weight percent titanium dioxide, and from about 0.1 to about 0.4 weight percent manganese dioxide, wherein the combined weight percent of strontium titanate and barium zirconate is from about 20 to about 28 percent by weight;

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 28 total)

PatentTitleYearCitations
US 5,378,662 AGlass, dielectric composition, multilayer wiring substrate, and multilayer ceramic capacitor199541
US 4,536,821 ACeramic capacitors and dielectric compositions198517
EP 0,156,489 A3Ceramic glass material, capacitor made therefrom and method of making the same—0
US 11,292,747 B2Barium strontium titanate-based dielectric ceramic materials, preparation method and application thereof20220
EP 1,978,004 A1Dielectric ceramic composition, complex electronic device and multilayer ceramic capacitor—0
US 2010297640 A1Hand held micro pcr device—20
US 4,524,098 ABoard for additive circuits19857
US 6,410,633 B1Antibacterial glass and resin composite comprising the same200221
US 5,431,955 AHigh frequency conductive material and resonator and method for making199511
WO 8,402,521 A1Low firing ceramic dielectric for temperature compensating capacitors—8
US 7,641,970 B2Dielectric particle aggregate comprising a surface layer of zinc titanate, low temperature sinterable dielectric ceramic composition using same20100
US 5,059,566 AHigh-dielectric constant ceramic composite and ceramic capacitor elements199122
US 5,378,663 AMethod of preparing a dielectric ceramic composition for producing a dielectric resonator or filter for microwave applications199511
US 5,672,378 AMethod for making a BaTiO3 powder mixture the powder mixture and method for making a Y5V ceramic body therefrom199728
US 2007172652 A1Dielectric particle aggregate, low temperature sinterable dielectric ceramic composition using same, low temperature sintered dielectric ceramic produced by using same—4