Abstract
A tire whose tread comprises as elastomer a styrene-butadiene or a styrene-isoprene co-polymer having a glass transition temperature above minus 50° C., said composition having a rebound resilience of 55% or more. The glass transition temperature is preferably between minus 40° C. and minus 25° C. and the rebound resilience is preferably between 60% and 70%.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 28.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A tire comprising sidewalls, beads, and a tread, whose tread composition having improved wet grip and rolling resistance is formed of an elastomer composition containing as the elastomer a styrene-butadiene copolymer or a styrene-isoprene copolymer, the unvulcanized polymer forming the elastomer having a glass transition temperature of above about minus 50° C. to about minus 20° C., and said vulcanized tread composition having a rebound resilience of about 55% to about 95% measured using the Dunlop Pendulum at 50° C., according to B.S. 903/1950.
- Claim 2Depends on #1
A tire according to claim 1, in which said glass transition temperature is in the range from minus 45° C. to minus 20° C.
- Claim 3Depends on #2
A tire according to claim 2, in which said glass transition temperature is in the range from minus 40° C. to mi
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 28 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (1)
- Peterson, Jr. et al. "Tread Compound Effects in Tire Traction" in The Physics of Tire Traction Edited by Hayes et al., p. 229, Plenum Press, Oct. 1974, 1973.