Patents
US 4,333,902 A#468683 Most CitedExpiredUnited States (USPTO)Utility

Process of producing a sintered compact

72Forward Citations (#468683 Global)
1.6/yrCitation Velocity (#2991422 Global)
6.32Citation PageRank (#2261089 Global)
4Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process of producing a sintered compact comprises filling a cup with a powdered material to be sintered, putting on an opening of the cup a covering member consisting of a lid and solder so as to permit ventilation between the interior and exterior of the cup to form a cup assembly, applying heat as well as vacuum to the cup assembly to degas the powdered material, melting the solder by the continuation of heat to air-tightly seal the cup with the lid to obtain a closed cup compressible under high pressure at high temperature while maintaining the air-tight seal, and hot-pressing the closed cup to obtain a sintered compact. The covering member may include a porous lid closing the cup and a solder put on the porous lid.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 72.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Process of producing a sintered compact comprising: filling a cup with a powdered material to be sintered; putting on an opening of the cup a covering member consisting of a lid and solder so as to permit ventilation between the interior and exterior of the cup to form a cup assembly; applying heat as well as vacuum to the cup assembly to degas the powdered material; melting the solder by the continuation of heat to air-tightly seal the cup with the lid to obtain a closed cup compressible under high pressure at high temperature while maintaining the air-tight seal; and hot-pressing the

  2. Claim 2Depends on #1

    Process of producing a sintered compact as claimed in claim 1, wherein said covering member comprises a porous lid closing the cup and a solder put on said porous lid.

  3. Claim 3Independent Claim

    Proce

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • Stromberg et al., "Sintering of Diamond at 1800.degree.-1900.degree. C. and 60-65 K bar," Cev. Bull., vol. 49, No. 12, (1970).
  • Stromberg et al., "Sintering of Diamond at 1800°-1900° C. and 60-65 K bar," Cev. Bull., vol. 49, No. 12, (1970).