Patents
US 4,331,631 A#580683 Most CitedExpiredUnited States (USPTO)Utility

Enhanced oxide whisker growth on peeled Al-containing stainless steel foil

64Forward Citations (#580683 Global)
1.4/yrCitation Velocity (#3703537 Global)
13.01Citation PageRank (#685120 Global)
5Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

In the preferred embodiment, a method is disclosed for preparing a metal foil composed of a ferritic stainless steel alloy and having a surface that is substantially covered by high aspect alumina whiskers. The preferred foil alloy comprises 15 to 25 weight percent Cr, 3 to 6 weight percent Al, 0.3 to 1.0 weight percent Y and the balance Fe. The method comprises forming the foil by a metal peeling process and treating the foil by heating in air at a temperature between about 870° C. and about 930° C. for a time sufficient to grow the alumina whiskers. In a particularly useful embodiment, the whisker-covered foil is coated with a noble metal-impregnated alumina layer and wound into a suitable cylindrical structure for use as a monolith-type catalytic converter for automotive exhaust gas treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 64.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a metal foil of an aluminum-containing ferritic stainless steel alloy having densely spaced oxide whiskers on a surface thereof, said method comprising forming by a metal peeling process a severely worked foil having an irregular surface, and heating the peeled foil in an oxygen-containing gas at a temperature and for a time sufficient to form said oxide whiskers on said surface.

  2. Claim 2Independent Claim

    A method of forming a metal foil of a ferritic stainless steel alloy containing 15 to 25 weight percent Cr, 3 to 6 weight percent Al, optionally 0.3 to 1.0 weight percent Y and the balance Fe, said foil having densely spaced oxide whiskers on a surface thereof, said method comprising forming by metal peeling a severely cold-worked foil hav

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Tien et al., "Mechanism of Oxide Adherence on Fe-25Cr-4Al (Y or Sc) Alloys", Metallurgical Transactions, vol. 3, Jun. 1972, pp. 1587-1599.