Abstract
A steel strip displaying high strength and formability properties is fabricated by coiling a steel strip which has been previously processed through a hot-strip mill from an initial steel having a very low amount of alloying compounds and having a temperature of between 750° and 900° C., the coiled steel strip being maintained at a temperature of between 800° and 650° C. for a period of at least one minute, and thereafter cooled to a temperature of below 450° C., the cooling being accomplished at a rate exceeding 10° C./second.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 12.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of forming a steel strip which displays high strength and formability properties, the steel in said steel strip comprising a dual-phase steel containing mostly fine-grained ferrite with grains of martensite dispersed therein, which method comprises (a) processing an initial steel which comprises 0.05-0.20% carbon, 0.50-2.0% silicon, 0.50-1.5% manganese, 0-1.5% chromium, 0-0.15% vanadium, 0-0.15% molybdenum, 0-0.04% titanium, 0-0.02% niobium, balance of iron and normal impurities through a hot-strip mill so as to form a hot steel strip, (b) cooling the hot steel strip of step (a) to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗