Dimensionally stabilized imaging element and method
Abstract
A thermally processable imaging element and method are disclosed, wherein dimensional changes after thermal processing for about 5 seconds at a temperature of about 125° C., do not exceed ±0.03%. The imaging element features an amine-generating and an amine-responsive composition. The method features preheating the element prior to exposure to dimensionally stabilize it.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A thermally processable photographic imaging element comprising a polymeric film support having dimensional changes that are no greater than ±0.1% in width and length when heated in an uncoated state for about 5 seconds at a temperature of about 125° C., and on the support, at least one radiation-sensitive layer comprising a radiation-responsive, amine-generating composition that includes a reducible cobalt(III) complex containing releasable amine ligands, and an amine-responsive dye precursor, said element having as an essential property, an overall thermal-reaction hysteresis that will p
- Claim 2Independent Claim
A thermally processable photographic imaging element comprising a polymeric film supp
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,171,758 B1 | Dimensionally stable flexographic printing plates | 2001 | 32 |
References Cited — Backward Prior Art (10)
Non-Patent Literature (3)
- Research Disclosure, Pub. 16239, Published Oct. 1977, in vol. 162.
- Research Disclosure, Pub. 17935, Published Mar. 1979, in vol. 179.
- Research Disclosure, Pub. 18436, Published Aug. 1979, in vol. 184.