Method for making iron-metalloid amorphous alloys for electromagnetic devices
Abstract
An amorphous metal alloy which is at least 90 percent amorphous and consists essentially of a composition having the formula FeaBbSicCd wherein "a", "b", "c" and "d" are atomic percentages ranging from about 80.0 to 82.0, 12.5 to 14.5, 2.5 to 5.0 and 1.5 to 2.5, respectively, with the proviso that the sum of "a", "b", "c" and "d" equals 100, is annealed at a temperature ranging from 380 DEG -410 DEG C. The resulting alloy has decreased high frequency core losses and increased low field permeability; is particularly suited for high frequency applications.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 43.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of enhancing the magnetic properties of a metal alloy which is at least 90 percent amorphous and consisting essentially of a composition having the formula Fe a B b Si c C d wherein "a", "b", "c" and "d" are atomic percentages ranging from about 80.0 to 82.0, 12.5 to 14.5, 2.5 to 5.0 and 1.5 to 2.5, respectively, with the proviso that the sum of "a", "b", "c" and "d" equals 100, which method comprises the step of annealing said alloy at a temperature ranging from about 380°-410° C.
- Claim 2Depends on #1
A method as recited in claim 1, wherein said annealing step further comprises: (a) heating said alloy to a temperature sufficient to achieve stress relief; (b) cooling said alloy at a rate of about 0.5° C./min to 75° C./min; and (c) applying a magnetic field to said alloy during sa
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗