Patents
US 4,298,403 A#7167470 Most CitedExpiredUnited States (USPTO)Utility

Ion-implanted evaporated germanium layers as n+ contacts to GaAs

13Forward Citations (#7167470 Global)
0.3/yrCitation Velocity (#25906160 Global)
13.50Citation PageRank (#644630 Global)
4Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of forming a single, reliable n + contact for discrete GaAs devices. A film of p-type Ge is deposited uniformly over the surface of a n-type GaAs substrate. Ions of phosphorous or arsenic are implanted to 5×10 18 ions/cc at a depth of 1500 A. The ends and the sides of the substrate and Ge layer are capped by a CVD oxide and annealed at 450°-500° C. for about one hour. This process over-compensates the initial p-type layers which results in the Ge layer becoming n + . The oxide is removed by an etch process and the n + Ge is etched to form two separate contact sections of n + Ge. The n + Ge is then metalized to form ohmic contacts by use of NiAu. A CVD oxide overcoat may again be applied and annealed at about 500° C. to drive a shallow 200-500 A, n + germanium diffusion into the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for forming n + contacts for GaAs devices which comprises: depositing a p-type Ge film onto a GaAs substrate, implanting ions of arsenic or phosphorous into said Ge film to a desired depth, capping said Ge film on the top and sides and on the sides of the GaAs substrate with an oxide, annealing said capped Ge film-GaAs substrate in an inert gas ambient at a sufficient temperature over a sufficient time period to over-compensate the p-type Ge layer to change the p-type layer to an n + layer, removing the oxide cap, etching said n + Ge film to form contact areas, and depo

  2. Claim 2Depends on #1

    A method as claimed in claim 1 in which: said GaAs substrate is desorbed at a temperature of about 575° C. for about 15 m

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (4)

  • Itoh et al., J. Appl. Phys., 42, (1971), 5120.
  • Jaros et al., Solid State Electronics, 18, (1975), 1029.
  • Rao et al., J. Appl. Phys., 49, (1978), 3898.
  • Woodall et al., IBM-TDB, 10, (1968), 1476.